Polyester yarns
Textured yarns
Application: Production of various textiles: lining, apparel textiles, furniture fabrics, jacquard fabrics, fabrics for automotive industry, gobelins, technical fabrics, awning fabrics, stockinet cloths, hosiery, fabrics for haberdashery: hangings and laces, gloves, carpets, ropes, tapes, basis for artificial fur, needlepunched materials and so on.
Packing: in carton boxes (760x380x304 mm), 8 bobbins per box.
Raw-white untwisted: tex 5,5 f 32, 7,6 f 32, 8,3 f32, 9,2 f 32, 12 f 32, 16 f 48, 16,7 f48, 18,5 f 48
Raw-white air-entangled: tex 9,2 f 32, 12 f 32, 16 f 48, 16,7 f48, 18,4 f64, 18,5 f 48, 22,2 f 64, 24,5 f 64, 33,4 f 96, 37,2 f 96
Raw-white twisted: tex 25 f 64, 33,4 f 96, 37,5 f 96
Dyed untwisted: tex 8,5 f 32, 9,3 f 32, 12,5 f 32, 16,3 f 48, 17 f 48, 18,8 f 48
Dyed air-entangled: tex15,5 f 64, 19 f 48, 25,4 f 64, 38,5 f 96
Dyed twisted: tex25,4 f 64, 38,2 f 96
For carpets and textile haberdashery raw white: 18,5 tex, 34 tex, 37,0 f 96 è f 128, 36 tex, 48,7 tex, 25 f 64, 27 f 96, 37 f 96, 48 f 144
For carpets and textile haberdashery dyed: 18,8 tex f 64, 25,4 tex f 64, 37 tex f 96, 38,2 tex, 48,7 tex
Physical properties
Qualitative cgaracteristics* | Raw white | Air-entangled TP RB 400031289.190-2003 |
Dyed | For carpets and textile haberdashery | ||
Untwisted | Twisted | Raw white | Dyed | Untwisted and Twisted | Raw white and Dyed | |
Unit breaking load, mN/tex, min | 290 | 290 | 280 | 280 | 290 | 280 |
Elongation at break, % | 24 +5 | 25 + 5 | 24 + 4 | 24 + 5 | 25+5 | 24+5 |
Variation coefficient in elongation at break, %, max | 12 | 13 | 13 | 13 | 13 | – |
Deviation of actual linear density from nominal one, %, max | 2 | 2,5 | 2,5 | 2,5 | 2 -3 |
2,5 |
Variation coefficient in linear density, %, max | 2,5 | 2,5 | – | – | – | – |
Degree of crimp – for 12 tex – for 9,2 tex |
16+3 26+3 20+3 |
14+3 | – | – | 3,5-7,5 | – |
Crimp stability, % min | 65 | 63 | – | – | 55 | – |
Number of knots per 1 m, min | – | – | 100 | 100 | – | – |
Oil content, % | 0,8-3,8 | 0,8-3,8 | 0,7-4 | 0,7-4 | 0,8-3,8 | 04-sty |
Number of twists per 1 m | 65+10; 120+10 | – | – | 60+10, 120+10 | 65+10; 40+10 | |
Linear shrinkage, % | 6 | 6 | 6 | – | – | – |
Bobbin weight, g for tex 9,3 12,5 and 38,2 for tex 18,8 and 25,4 |
2800+200 – – |
2500+200 2200+200 (120 TPM) – |
2500+200 – – |
2400+200 – – |
– 2300+200 2400+200 |
2500+300 |
Characteristics are indicated: for raw white yarn — grade “A”, for dyed yarns – grade “B”.
Polyester yarns are produced on cross-wound polypropylene cylindrical tubes.