Application: Production of various textiles: lining, apparel textiles, furniture fabrics, jacquard fabrics, fabrics for automotive industry, gobelins, technical fabrics, awning fabrics, stockinet cloths, hosiery, fabrics for haberdashery: hangings and laces, gloves, carpets, ropes, tapes, basis for artificial fur, needlepunched materials and so on. Packing: in carton boxes (760x380x304 mm), 8 bobbins per box. Raw-white untwisted: tex 5,5 f 32, 7,6 f 32, 8,3 f32, 9,2 f 32, 12 f 32, 16 f 48, 16,7 f48, 18,5 f 48 Raw-white air-entangled: tex 9,2 f 32, 12 f 32, 16 f 48, 16,7 f48, 18,4 f64, 18,5 f 48, 22,2 f 64, 24,5 f 64, 33,4 f 96, 37,2 f 96 Raw-white twisted: tex 25 f 64, 33,4 f 96, 37,5 f 96 Dyed untwisted: tex 8,5 f 32, 9,3 f 32, 12,5 f 32, 16,3 f 48, 17 f 48, 18,8 f 48 Dyed air-entangled: tex15,5 f 64, 19 f 48, 25,4 f 64, 38,5 f 96 Dyed twisted: tex25,4 f 64, 38,2 f 96 For carpets and textile haberdashery raw white: 18,5 tex, 34 tex, 37,0 f 96 è f 128, 36 tex, 48,7 tex, 25 f 64, 27 f 96, 37 f 96, 48 f 144 For carpets and textile haberdashery dyed: 18,8 tex f 64, 25,4 tex f 64, 37 tex f 96, 38,2 tex, 48,7 tex

Physical properties

Qualitative cgaracteristics* Raw white Air-entangled TP RB 400031289.190-2003 Dyed For carpets and textile haberdashery
Untwisted Twisted Raw white Dyed Untwisted and Twisted Raw white and Dyed
Unit breaking load, mN/tex, min 290 290 280 280 290 280
Elongation at break, % 24 +5 25 + 5 24 + 4 24 + 5 25+5 24+5
Variation coefficient in elongation at break, %, max 12 13 13 13 13
Deviation of actual linear density from nominal one, %, max 2 2,5 2,5 2,5 2 -3 2,5
Variation coefficient in linear density, %, max 2,5 2,5
Degree of crimp –          for 12 tex –          for 9,2 tex 16+3 26+3 20+3 14+3 3,5-7,5
Crimp stability, % min 65 63 55
Number of knots per 1 m, min 100 100
Oil content, % 0,8-3,8 0,8-3,8 0,7-4 0,7-4 0,8-3,8 04-sty
Number of twists per 1 m 65+10; 120+10 60+10, 120+10 65+10; 40+10
Linear shrinkage,  % 6 6 6
Bobbin weight, g for  tex 9,3 12,5  and 38,2 for tex 18,8 and 25,4 2800+200 – – 2500+200 2200+200 (120 TPM) – 2500+200 – – 2400+200 – –  – 2300+200 2400+200 2500+300